Reslin® stands out as the very first 100% biodegradable plant-based resin, subtly combining innovation and respect for the environment.
Its formulation based on linseed oil and a plant-based activator gives it a reduced ecological footprint, positioning Reslin as THE new eco-responsible alternative to traditional epoxy resins.
Malleable and versatile, Reslin is ideal for all creative types, and lends itself easily to the incorporation of pigments and decorative fillers, paving the way for unique and varied visual renderings.
Used on its own, it offers remarkable flexibility, while the addition of fillers gives it the rigidity and strength needed for long-lasting creations.
To enhance your creations and increase their performance, integrate natural materials such as Glassroxx, stones, Terrazzo Jesmonite or other small, fine aggregates. The smaller the particle size, the greater the resistance.
Compatible with a wide variety of pigments and mineral fillers, Reslin can also be blended with natural elements such as herbs, coffee or dried flowers for a refined, organic look. However, be careful not to use water-based additives (acrylics) to preserve the integrity of its oil-based formulation.
Mixing ratio 2:1 (100 g Reslin oil to 50 g activator)
Color: translucent amber
Reheating of components and additive: 20 min. at 60°C
Resin + activator mixture: 2-3 min.
Pot life: 15 min.
Resting time before cooking: 20 min.
Cooking: phase 1: 20 min. at 90°C (200°F), phase 2: 20 min. at 120°C (250°F)
Demoulding: when properly cooled
Compatibility: GlassRoxx, mica powder, flakes, Terrazzo, etc.DO NOT USE water-based additives!
100% biodegradable
Free from harmful substances
Suitable for children
Environmentally-friendly alternative to epoxy
For use with bare hands
Circular product
Ready to use after just 12 hours
Suitable for small and large objects
1. Prepare quantities
Mixing ratio 1:2.
Measure 1 part Reslin activator to 2 parts Reslin oil.
2. Prepare components Reslin
It is very important to bring the Reslin components to the right temperature before use. Heat the activator and Reslin oil separately in an oven for 20 minutes at 60°C (140°F). If the addition of Glassroxx or other additives is desired, they can also be reheated so as not to precipitate the cooling of the resin. DO NOT USE A MICROWAVE OVEN.
3. Mixture A+B
Pour the Reslin oil into the activator and stir the mixture thoroughly for several minutes. You can then add additives to the Reslin mixture, such as GlassRoxx, mica powder, flakes, etc.
4. Filling the mould.
How to proceed depends on the composition of your mix. Reslin reinforced with decorative aggregates should be poured and then packed. After filling the mold, let the mixture rest for 20 minutes before placing in the oven.
5. Baking Reslin in 2 phases
Phase 1: Place your product in a fan-assisted oven and heat for 20 minutes at 90°C.
Phase 2: increase temperature to 120°C and reheat for a further 20 minutes.
6. Cooling and demolding
After the second heating phase, the object can be cooled immediately. Let the object cool in the open air or place the mold in cold water. Make sure the object has cooled down completely before removing it from the mold. It will take 12 hours for your Reslin object to harden completely and be ready for use.
RUE J. VAN HOVE, 35 1950 KRAAINEM